Gold alloys

Au 750 2N

Au 750 2N

 Colour:  light yellow
 Vickers
 Hardness:
 120 HV, annealed
 Melting range:  905 - 960°C
 Fineness:  750 Au, Ag
 Comments:  General
 Application

 

Au 750 3N

Au 750 3N

 Colour:  Deep yellow
 Vickers
 Hardness:
 135 HV, annealed
 Melting range:  870 - 905°C
 Fineness:  750 Au, Ag
 Comments:  General
 Application

 

 

Au 750 4N

Au 750 4N

 Colour:  Rose
 Vickers
 Hardness:
 160 HV, annealed
 Melting range:  885 - 915°C
 Fineness:  750 Au, Ag
 Comments:  General
 Application

 

 

Au 750 5N

Au 750 5N

 Colour:  Red
 Vickers
 Hardness:
 155 HV, annealed
 Melting range:  875 - 900°C
 Fineness:  750 Au, Ag
 Comments:  General
 Application

 

 

Au 750 6N

Au 750 6N

 Colour:  Red
 Vickers
 Hardness:
 160 HV, annealed
 Melting range:  880 - 920°C
 Fineness:  750 Au, Ag, Pt
 Comments:  General
 Application

 

 

Au 917

Au 917

 Colour:  Deep yellow
 Vickers
 Hardness:
 85 HV, annealed
 Melting range:  970 - 990°C
 Fineness:  917 Au, Ag
 Comments:  General
 Application

 

 

Au 750 Pd 125

Au 750 Pd 125

 Colour:  White
 Vickers
 Hardness:
 125 HV, annealed
 Melting range:  1060 - 1135°C
 Fineness:  750 Au, Pd, Ag
 Comments:  General
 Application

 

Au 750 Pd 124 Guss

Au 750 Pd 124 Guss

 Colour:  White
 Vickers
 Hardness:
 150 HV, annealed
 Melting range:  1045 - 1110°C
 Fineness:  751 Au, Pd, Ag
 Comments:  Casting alloy
 without Ni

 

Au 750 Pd 160

Au 750 Pd 160

 Colour:  White
 Vickers
 Hardness:
 135 HV, annealed
 Melting range:  1065 - 1150°C
 Fineness:  750 Au, Pd
 Comments:  General
Application

 

Au 760 Ni

Au 760 Ni

 Colour:  White
 Vickers
 Hardness:
 165 HV, annealed
 Melting range:  1100 – 1150°C
 Fineness:  760 Au, Pd, Ni
 Comments:  Hard alloy

 

Au 999.9

Au 999.9

 Colour:  Deep yellow
 Vickers
 Hardness:
 65 HV, annealed
 Melting range:  1063°C
 Fineness:  999.9 Au
 Comments:  Fine gold

 

Fairtrade Alloys

Au 750 3N Fairtrade

Au 750 3N Fairtrade

 Colour:  Deep yellow
 Vickers
 Hardness:
 135 HV, annealed
 Melting range:  870 - 905°C
 Fineness:  750 Au, Ag
 Comments:  Fairtrade alloy

 

Au 750 4N Fairtrade

Au 750 4N Fairtrade

 Colour:  Rose
 Vickers
 Hardness:
 160 HV, annealed
 Melting range:  885 - 915°C
 Fineness:  750 Au, Ag
 Comments:  Fairtrade alloy

 

Au 750 5N Fairtrade

Au 750 5N Fairtrade

 Colour:  Red
 Vickers
 Hardness:
 155 HV, annealed
 Melting range:  875 - 900°C
 Fineness:  750 Au, Ag
 Comments:  Fairtrade alloy

 

Au 750 Pd 125 Fairtrade

Au 750 Pd 125 Fairtrade

 Colour:  White
 Vickers
 Hardness:
 160 HV, annealed
 Melting range:  1060 -1125°C
 Fineness:  750 Au, Ag, Pd
 Comments:  Fairtrade alloy

 

Au 750 Pd 160 Fairtrade

Au 750 Pd 160 Fairtrade

 Colour:  White
 Vickers
 Hardness:
 135 HV, annealed
 Melting range:  1065 - 1150°C
 Fineness:  750 Au, Pd
 Comments:  Fairtrade alloy

 

Au 999.5 Fairtrade

Au 999.5 Fairtrade

 Colour:  Deep yellow
 Vickers
 Hardness:
 65 HV, annealed
 Melting range:  1063°C
 Fineness:  999.5 Au
 Comments:  Fairtrade alloy

 

Platinum alloys

Pt 950 Ru

Pt 950 Ru

 Colour:  White
 Vickers
 Hardness:
 130 HV, annealed
 Melting range:  1725 - 1745°C
 Fineness:  950 Pt, Ru
 Comments:  General
 Application,
 good machine
 processing

 

Palladium alloys

Pd 950 Ru Ga

Pd 950 Ru Ga

 Colour:  White
 Vickers
 Hardness:
 125 HV, annealed
 Melting range:  1500 - 1520°C
 Fineness:  950 Pd, Ru, Ga
 Comments:

 General
 Application
 suitable for
 casting

 

Pd 500

Pd 500

 Colour:  White
 Vickers
 Hardness:
 130 HV, annealed
 Melting range:  1150 - 1220°C
 Fineness:  500 Pd, Ag, Cu
 Comments:  General
 Application

 

Silver alloys

Ag 925

Ag 925

 Colour:  White
 Vickers
 Hardness:
 70 HV, annealed
 Melting range:  805 - 890°C
 Fineness:  925 Ag, Cu
 Comments:  General
 Application

 

Sterling+

Sterling+

 Colour:  White
 Vickers
 Hardness:
 60 HV, annealed
 Melting range:  890 - 940°C
 Fineness:  972 Ag
 Comments:  Tarnish resistant
 silver alloy

 

Ag 999.0

Ag 999.0

 Colour:  White
 Vickers
 Hardness:
 26 HV, annealed
 Melting range:  962°C
 Fineness:  999.9 Ag
 Comments:  Fine silver